dc.description.abstract Styrene, ethyl benzene and cis-polybutadiene (for high impact grade) are added and kept in a dissolver for 6-8 hours to ensure a complete dissolution of the rubber. This mixture is filtered and fed to the first of two reactors maintained at l120C where the conversion is 8.7 (maintaining the solution beyond the phase inversion point). In the second reactor, 95 r percent of the styrene is converted by the end of the react ion, when the temperature has risen to about 1650C. Polymerisation is completed in a finishing column held at 2200C for 1-2 hours followed by cooling, extrusion and pelletising. en_US
dc.language.iso en en_US
dc.publisher United Nations Industrial Development Organization en_US
dc.subject Polystyrene en_US
dc.title Polystyrene en_US
dc.type Other en_US


Files in this item

This item appears in the following Collection(s)

Show simple item record

Search EDII IR


Advanced Search

Browse

My Account