dc.description.abstract The styrene and butadiene monomers are mixed in an emulsion reactor with water, catalyst emulsifier (soap) and molecular weight modifier (eg tertdodecy mercaptan). The polymerisation temperature is low at SoC. The conversion limit is 60 percent to prevent gel formation, this will typically be achieved in 12-15 hours. Butadiene and styrene are removed from the latex by vacuum and steam stripping respectively and recycled after purification. The product rubber is recovered by coagu 1at i ng the latex, dewatered and dried. en_US
dc.language.iso en en_US
dc.publisher United Nations Industrial Development Organization en_US
dc.subject SBR en_US
dc.subject Cold Emulsion Process en_US
dc.title SBR-Cold Emulsion Process en_US
dc.type Other en_US


Files in this item

This item appears in the following Collection(s)

Show simple item record

Search EDII IR


Advanced Search

Browse

My Account